High Temperature Differential Scanning Calorimeter DH-DSC-550C
Product introduction
DSC is a differential display with the highest accuracy launched by Hongtuo. The sensor is made of imported material, with high sensitivity. The signal acquisition circuit is shielded and protected, with strong anti-interference and high baseline stability.
The differential scanning calorimeter is a touch screen type, which can be used for glass transition temperature test, phase transition test, melting and enthalpy value test, product stability test, curing test, specific heat test, oxidation induction period test, etc. Wide application scope.
Technical parameter
1. Temperature range: room temperature 1550
2. Temperature resolution: 0.001
3. Temperature fluctuation: 0.01
4. Temperature repeatability: 0.1
5. Heating rate: 0.1100/min
6. Constant temperature time: program setting
7. Temperature control method: PID temperature control, heating, constant temperature (fully automatic program control)
8. DSC range: 0600mW
9. DSC resolution: 0.01uW
10. DSC sensitivity: 0.001mW
11. Working power supply: AC220V/50Hz or customized
12. Atmosphere control gas: nitrogen, oxygen (automatic switching of the instrument)
13. Gas flow: 0-300mL/min
14. Gas pressure: 0.2MPa
15. Display mode: 24bit color, 7-inch LCD touch screen display
16. Data interface: standard USB interface
17. Parameter standard: equipped with standard materials (indium, tin), users can calibrate the temperature by themselves
18. The instrument has multiple sets of thermocouples, one set for testing sample temperature, and one set for testing the internal ambient temperature of the instrument
19. The instrument has a multi-point calibration function, which can meet the precise testing of high, medium and low samples
20. The software can set the data acquisition frequency, and can export EXECL data packages and PDF reports
21. Curve scanning: temperature rise scanning, temperature drop scanning, constant temperature scanning
Price: